Tungsten trioxide powder applying for thermal insulation film may be prepared by hydrothermal synthesis method. For example, the Na2WO4 solution is acidified with HCl and hydrothermally reacted at 130~200°C for 1~5 days. Eventually, tungsten trioxide with uniform particle size distribution can be obtained. The obtained tungsten trioxide can be used for the preparation of a variety of heat-insulating materials, such as film, coating, and so on, thereby being applied to heat-insulating glasses and the like. What is hydrothermal synthesis? Hydrothermal…